We are almost done! Now that we have the image and it’s aligned to the mug, we secure it with Goldfinger tape. Since we use a heating press, we also have to use a specific type of tape, so we don’t have any complications. Then, we place the mug into the heating press, which is at 380- 400F. Therefore, we press the mug for about 4-5 min.